Polypropylene PP Mono Micro Synthetic Staple Fiber for Concrete Basic Info

  • Model NO.: ELT-PPFM

  • Function: Reinforce The Concrete

  • Certification: CE, ISO

  • Polypropylene Staple Fiber Crack Elongation: 20+/-5%

  • Fiber Diameter: 20-30um

  • Color: White

  • Feature: Anti-Cracking

  • Density: 0.91+/-0.01um

  • Polypropylene Staple Fiber Transport Package: 10/20kg Per Plastic Nonwoven Bag

  • Origin: Anhui

  • Type: Concrete Additive

  • Material: 100% Virgin PP

  • Application: Cement,Concrete, Motar

  • Polypropylene Staple Fiber Fiber Type: Monofilament

  • Tensile Strength(MPa): 450 Min.

  • Usage: Concrete

  • Polypropylene Staple Fiber Acid & Alkair Resistance: Strong

  • Specification: 0.6/0.9/1.0 kg per PE bag or paper bag

  • HS Code: 55034000

Polypropylene PP Mono Micro Synthetic Staple Fiber for Concrete Product Description


 
EltFiber-PPMF monofilament fiber was produced by referring foreign advanced technology for fiber spinning, modified by adding functional additive and special surface-treating. Mixing into cement concrete, it has many advantages such as good dispersing, better water affinity, strong linking force. It is suited to reinforce and crack-resist to every kinds of cement concrete and mortar, specially used in engineering of building surface, floor, wall etc…..

Polypropylene PP Mono Micro Synthetic Staple Fiber for Concrete Brief specification:
Compliance
ASTM C1116, Type III
BS EN 14889 - 2
1, Normal Type MicroFiber Monofilament PPMF-

Raw Material :PolypropyleneCrack Elongation:20+/-5%
Fiber Type :Monofilament PPMF-AFiber Diameter:20-30um
Melting Point(C Deg.) :160 - 170Density(g/cm3) :0.91+/-0.01
Acid &Alkali Resistance :StrongTensile Strength(MPa):450 min.
Length:Times of 4mm or 6mmWater absorbency :NO
Normal Length4mm, 6mm, 8mm, 12mm,18mm, 24mm, 30mm etc...
(times of 4mm or 6mm with 1mm more or less )


2. Special Type MicroFiber Monofilament
A. MicroFiber Monofilament PPMF-B:High Tensile Strength -----------600MPa Min
B. MicroFiber Monofilament PPMF-C:Superfine-------------------------20+/-2um Dia
C. MicroFiber Monofilament PPMF-D:High dispersion------------------Special Surface-Treating

Packing:

PP Fiber ShapeInner Packing
(PE film bag)
Outer Packing
(Plastic Woven bag)
20'gp40'HQ
Monofilament0.6/0.9/1.0 kg18/20kg10000kg20000kg
 Inner Packing
 (water Soluble paper bag)
Outer Packing 
(Carton)
  
Monofilament0.6/0.9/1.0 kg18/20kg8000kg16000kg



Polypropylene PP Mono Micro Synthetic Staple Fiber for Concrete Functions:
?Resist to shrink & crack            
?Increase seepage resistance
?Increase friction resistance          
?Increase freezing & thawing resistance                              
?Improve tendons protection         
?Replace steel net (using in plastering)
? Prevent mortar split and crackle expansion  
?Increase impact resistance and peeling resistance
 
Polypropylene PP Mono Micro Synthetic Staple Fiber for Concrete Advantages:
? Cost effective
? Replaces anti crack mesh reinforcement
? Decreases construction time and labor
? Inhibits intrinsic cracking in concrete                           
? Disperses uniformly throughout the mix
? Do not rust
? Explosive spall control
 
Polypropylene PP Mono Micro Synthetic Staple Fiber for Concrete Applications:
A). suit for the waterproof layer, floor, inner & outer wall of industrial and civil construction.
B). Increase cracking resistance on the surface of industrial workshop, warehouse and parking lot.
C). Increase cracking & seepage resistance of the ground in natatorium, swimming pool, pond and ditch.
D). Suit for any mortar projects and common concrete projects.
E). Highway, bridge and other roads.
 
Polypropylene PP Mono Micro Synthetic Staple Fiber for Concrete Applying Instruction:
A). Dosage:  for resist the common cracks on surfaces, 0.9kg/m3 fibers to cement mortar Is enough, and for increasing reinforce and seepage resist application 1.8kg/m3 is enough.
B). Stirring requirement: The proportion of cement, sand and aggregate is no need to be changed. Put cement, aggregate, additive and fiber together, then stir after adding enough water and time for stirring can be prolonged for 2~3 minutes in order to make the compound mix completely. Also it can be mixed with cement and other aggregates in advance, stirring by adding water at worksite before construction.